Sign In | Join Free | My disqueenfrance.com |
|
Categories | Nickel Alloy Plate |
---|---|
Brand Name: | Zhonggong Special Metallurgy |
Model Number: | GH4180 alloy |
Place of Origin: | China |
MOQ: | 100KG |
Price: | Price is negotiated based on the required specifications and quantity |
Payment Terms: | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
Supply Ability: | 5000 tons per month |
Delivery Time: | 5-8 working days, depending on the parameters required for negotiation |
Packaging Details: | Standard export packaging, or packaging as required |
Density: | ~8.3 g/cm³ |
Melting Point: | ~1390°C (2530°F) |
Thermal Conductivity: | ~11-13 W/m·K |
Yield Strength: | ~700 MPa (102 ksi) |
Ultimate Tensile Strength: | ~900 MPa (130 ksi) |
Elongation: | ~10% |
Hardness (Rockwell): | ~HRB 90-95 |
Applications: | Aerospace components, gas turbines, and high-temperature engines |
Certification: | ISO Certificate |
Company Info. |
Jiangsu Zhonggongte Metallurgical Technology Co., Ltd. |
Verified Supplier |
View Contact Details |
Product List |
GH4180 Alloy
GH4180 is a high-performance nickel-based superalloy designed for superior strength and oxidation resistance in extreme environments. It is specifically engineered for applications requiring high-temperature stability and durability.
Key Features:
GH4180’s unique combination of high strength, thermal stability, and corrosion resistance makes it an excellent choice for demanding applications in aerospace and industrial sectors.
This description highlights GH4180 alloy's key attributes and typical applications, providing a comprehensive overview of its performance and benefits.
Here’s a detailed composition table for GH4180 alloy:
Element | Content Range |
---|---|
Nickel (Ni) | Balance |
Chromium (Cr) | 19.0-21.0% |
Iron (Fe) | 9.0-11.0% |
Cobalt (Co) | 8.0-10.0% |
Molybdenum (Mo) | 2.0-3.0% |
Titanium (Ti) | 2.0-3.0% |
Aluminum (Al) | 1.0-2.0% |
Boron (B) | 0.005-0.015% |
This table provides a clear overview of GH4180 alloy's chemical composition, detailing the content ranges of its key elements.
![]() |